Allgemein
Property | Value |
---|---|
Dichte | 10.26 g/cm³ Show Supplier Material materials with Dichte of 10.26 g/cm³ |
Porosität | 1 % Show Supplier Material materials with Porosität of 1 % |
Mechanisch
Property | Value |
---|---|
Härte, Vickers | 92 - 109 [-] Show Supplier Material materials with Härte, Vickers of 92 - 109 [-] |
Elektrisch
Property | Value |
---|---|
spezifischer Widerstand | 3.63e-08 Ω·m Show Supplier Material materials with spezifischer Widerstand of 3.63e-08 Ω·m |
Technological properties
Property | ||
---|---|---|
Other | Diameter 10 mm by 2-5 mm disks. Diameter 15 mm by 2-5 mm disks Special shapes upon request. | |
Processing methods | E-Forged™ from powders |