Allgemein
Property | Value |
---|---|
Dichte | 2.47 g/cm³ Show Supplier Material materials with Dichte of 2.47 g/cm³ |
Porosität | 1 % Show Supplier Material materials with Porosität of 1 % |
Mechanisch
Thermisch
Property | Value |
---|---|
Koeffizient der thermischen Ausdehnung | 1.06e-05 - 1.23e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.06e-05 - 1.23e-05 1/K |
Technological properties
Property | ||
---|---|---|
Other | Diameter 10 mm by 2-10 mm disks. Diameter 15 mm by 2-10 mm disks. 20 x 10 x 2 to 6 mm heigh. Special shapes upon request. | |
Processing methods | E-Forged™ from powders |