Allgemein
Property | Value | Comment |
---|---|---|
Bio-based content | 20 % Show Supplier Material materials with Bio-based content of 20 % | |
50 % Show Supplier Material materials with Bio-based content of 50 % | ||
Dichte | 1.17 g/cm³ Show Supplier Material materials with Dichte of 1.17 g/cm³ | Calculated |
Mechanisch
Property | Value | Comment |
---|---|---|
Biegefestigkeit | 25 MPa Show Supplier Material materials with Biegefestigkeit of 25 MPa | ASTM D790 |
Biegemodul | 0.618 GPa Show Supplier Material materials with Biegemodul of 0.618 GPa | ASTM D790 |
Elastizitätsmodul | 0.65 GPa Show Supplier Material materials with Elastizitätsmodul of 0.65 GPa | ASTM D638 |
Zugfestigkeit | 16 MPa Show Supplier Material materials with Zugfestigkeit of 16 MPa | ASTM D638 |
Thermisch
Property | Value | Comment |
---|---|---|
Schmelzpunkt | 130 °C Show Supplier Material materials with Schmelzpunkt of 130 °C | ASTM D3418 |
Rheological Properties
Property | Value | Comment |
---|---|---|
Schmelzmassenflussrate | 1.3 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 1.3 g/10min | ASTM D1238 (190°C/10 kg) |
Technological properties
Property | ||
---|---|---|
Application areas | BioBlend® XD 22620 is designed for blow molding applications that require stress crack resistance, rigidity, and high impact strength. | |
Certifications | USDA Certified Bio-based product |