Allgemein
Property | Value | Comment |
---|---|---|
Bio-based content | 20 % Show Supplier Material materials with Bio-based content of 20 % | |
50 % Show Supplier Material materials with Bio-based content of 50 % | ||
Dichte | 1.17 g/cm³ Show Supplier Material materials with Dichte of 1.17 g/cm³ | Calculated |
Mechanisch
Property | Value | Comment |
---|---|---|
Biegemodul | 0.708 GPa Show Supplier Material materials with Biegemodul of 0.708 GPa | ASTM D790 |
Dehnung | 12 % Show Supplier Material materials with Dehnung of 12 % | ASTM D638 |
Elastizitätsmodul | 0.568 GPa Show Supplier Material materials with Elastizitätsmodul of 0.568 GPa | ASTM D638 |
Impact strength, Izod notched, ASTM | 47 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 47 J/m | ASTM D256 |
Zugfestigkeit | 19 MPa Show Supplier Material materials with Zugfestigkeit of 19 MPa | ASTM D638 |
Thermisch
Property | Value | Comment |
---|---|---|
Schmelzpunkt | 130 °C Show Supplier Material materials with Schmelzpunkt of 130 °C | ASTM D3418 |
Rheological Properties
Property | Value | Comment |
---|---|---|
Schmelzmassenflussrate | 0.56 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 0.56 g/10min | ASTM D1238 (190°C/5 kg) |
Technological properties
Property | ||
---|---|---|
Application areas | Used for final products requiring strength and plasticity, such as packaging. | |
Certifications | USDA Certified Bio-based product |