Allgemein
Mechanisch
Property | Value | Comment |
---|---|---|
Biegemodul | 0.31 GPa Show Supplier Material materials with Biegemodul of 0.31 GPa | ASTM D790 |
Dehnung | 110 % Show Supplier Material materials with Dehnung of 110 % | ASTM D638 |
Elastizitätsmodul | 0.239 GPa Show Supplier Material materials with Elastizitätsmodul of 0.239 GPa | ASTM D638 |
Zugfestigkeit | 12 MPa Show Supplier Material materials with Zugfestigkeit of 12 MPa | ASTM D638 |
Thermisch
Property | Value | Comment |
---|---|---|
Schmelzpunkt | 140 - 160 °C Show Supplier Material materials with Schmelzpunkt of 140 - 160 °C | ASTM D3418 |
Rheological Properties
Property | Value | Comment |
---|---|---|
Schmelzmassenflussrate | 2.9 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 2.9 g/10min | ASTM D1238 (190°C/2.16 kg) |
Technological properties
Property | ||
---|---|---|
Application areas | NuPlastiQ® BC 27250 is intended for bags and film applications that require at least 40% bio-content. Used for products that require biodegradation and are intended for compost environments. | |
Certifications | USDA Certified Bio-based product |