Allgemein
Property | Value |
---|---|
Porosität | 4.0 % Show Supplier Material materials with Porosität of 4.0 % |
Schüttdichte | 3.55 g/cm³ Show Supplier Material materials with Schüttdichte of 3.55 g/cm³ |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminium | 99.5 % Show Supplier Material materials with Aluminium of 99.5 % | Al₂O₃ |
Andere | 0.025 Show Supplier Material materials with Andere of 0.025 | max. Magnetic Iron |
Eisen | 0.08 % Show Supplier Material materials with Eisen of 0.08 % | Fe₂O₃ |
Kalzium | 0.02 % Show Supplier Material materials with Kalzium of 0.02 % | CaO |
Natrium | 0.04 - 0.3 % Show Supplier Material materials with Natrium of 0.04 - 0.3 % | Na₂O | for Alfa tab 06 | alfa tab 30 respectively |
Silizium | 0.04 Show Supplier Material materials with Silizium of 0.04 | SiO₂ |
Technological properties
Property | ||
---|---|---|
Application areas | GNPGraystar’s Tabular Alumina is a raw material used in the manufacture of high alumina refractories, kiln furniture, electrical insulators, catalyst support media, investment casting, and more. |