Chemical properties
Property | Value | Comment |
---|---|---|
Aluminium | 0.1 Show Supplier Material materials with Aluminium of 0.1 | max. Al₂O₃ |
Eisen | 0.04 Show Supplier Material materials with Eisen of 0.04 | max. Fe₂O₃ |
Silizium | 0.1 Show Supplier Material materials with Silizium of 0.1 | max. SiO₂ |
Titan | 0.13 Show Supplier Material materials with Titan of 0.13 | max. TiO₂ |
Zirkonium | 99 % Show Supplier Material materials with Zirkonium of 99 % | min. ZrO₂ |
Technological properties
Property | ||
---|---|---|
Application areas | GNPGraystar’s Fused Monoclinic Zirconia Powder is excellent in metallurgical refractories such as zirconia nozzles and slide gates. It is also used in other refractories, ceramic pigments, auto brake additives, setting sands, and more. | |
Other | Particle size: Hollow Spheres or Customized |