Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 5.6 g/cm³ Show Supplier Material materials with Dichte of 5.6 g/cm³ | |
5.7 g/cm³ Show Supplier Material materials with Dichte of 5.7 g/cm³ | ||
Schüttdichte | 1.2 - 1.3 g/cm³ Show Supplier Material materials with Schüttdichte of 1.2 - 1.3 g/cm³ | ANSI B74.4 |
Mechanisch
Thermisch
Property | Value |
---|---|
Schmelzpunkt | 2550.0 °C Show Supplier Material materials with Schmelzpunkt of 2550.0 °C |
Chemical properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Aluminium | 0.8 % Show Supplier Material materials with Aluminium of 0.8 % | ANSI B74.14 | Al₂O₃ |
Eisen | 0.05 % Show Supplier Material materials with Eisen of 0.05 % | ANSI B74.14 | Fe₂O₃ |
Kalzium | 3.8 % Show Supplier Material materials with Kalzium of 3.8 % | ANSI B74.14 | CaO |
Silizium | 0.4 % Show Supplier Material materials with Silizium of 0.4 % | ANSI B74.14 | SiO₂ |
Titan | 0.1 % Show Supplier Material materials with Titan of 0.1 % | ANSI B74.14 | TiO₂ |
Zirkonium | 94.85 % Show Supplier Material materials with Zirkonium of 94.85 % | ANSI B74.14 | ZrO₂+HfO₂ |
Technological properties
Property | ||
---|---|---|
Application areas | GNPGraystar’s Fused Calcia-Stabilized Bubble Zirconia is used in the production of lightweight refractory bricks and castables, as loose bulk backup insulation for high temperature induction and nitriding furnaces, and other applications that require high temperature usage, rapid heating and cooling, and chemical stability. | |
Color | Yellow | |
Crystal structure | Cubic & Monoclinic Mixture | |
Other | Various sizes available. Custom sizes are also availble upon request. |