Property | Value | Comment |
---|---|---|
Loss on Ignition | 0.1 % Show Supplier Material materials with Loss on Ignition of 0.1 % | max. |
Partikelgröße D50 | 1.0 - 125.0 μm Show Supplier Material materials with Partikelgröße D50 of 1.0 - 125.0 μm | different specifications, please refer to the table below |
Partikelgrößenbereich | 2.0 - 120.0 µm Show Supplier Material materials with Partikelgrößenbereich of 2.0 - 120.0 µm | different specifications, please refer to the table below |
Relative Dichte | 3.8 [-] Show Supplier Material materials with Relative Dichte of 3.8 [-] | |
Spezifische Oberfläche | 0.02 - 1.2 m²/g Show Supplier Material materials with Spezifische Oberfläche of 0.02 - 1.2 m²/g | BET, different specifications, please refer to the table below |
Elektrisch
Property | Value |
---|
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminium | 99.8 % Show Supplier Material materials with Aluminium of 99.8 % | min. Al₂O₃ |
Eisen | 0.02 Show Supplier Material materials with Eisen of 0.02 | Fe₂O₃ |
Natrium | 0.005 Show Supplier Material materials with Natrium of 0.005 | Na⁺ |
0.02 Show Supplier Material materials with Natrium of 0.02 | max. Na₂O | |
Silizium | 0.05 Show Supplier Material materials with Silizium of 0.05 | SiO₂ |
Technological properties
Property | ||
---|---|---|
Application areas | GNPGraystar’s Spherical Alumina is used in resins, rubbers, and plastics as fillers for thermal conductive sheets, fillers for molding materials, base powder for baking ceramics, blasting materials, and spacers. | |
Color | White, Whitness: 90 | |
Other | Typical Sizing Specifications: Other/Special Sizing is available upon request. Actual PSD & SSA also available upon request. |