Allgemein
Property | Value | Comment |
---|---|---|
Anhydrous Solids Content | 78 % Show Supplier Material materials with Anhydrous Solids Content of 78 % | 1h/800°C |
82 % Show Supplier Material materials with Anhydrous Solids Content of 82 % | 1h/800°C | |
Partikelgröße D50 | 3.0 - 5.0 μm Show Supplier Material materials with Partikelgröße D50 of 3.0 - 5.0 μm | |
Partikelgrößenbereich | 1.0 - 10.0 µm Show Supplier Material materials with Partikelgrößenbereich of 1.0 - 10.0 µm | min. 90% |
Schüttdichte | 0.28 - 0.38 g/cm³ Show Supplier Material materials with Schüttdichte of 0.28 - 0.38 g/cm³ | |
Sieve residue 45μm | 0 % Show Supplier Material materials with Sieve residue 45μm of 0 % | |
Water content | 18 % Show Supplier Material materials with Water content of 18 % | |
22 % Show Supplier Material materials with Water content of 22 % | ||
pH-Wert | 11.0 - 12.0 [-] Show Supplier Material materials with pH-Wert of 11.0 - 12.0 [-] | 5% Slurry |
Optisch
Property | Value | Comment |
---|---|---|
Reflectance | 94.0 [-] Show Supplier Material materials with Reflectance of 94.0 [-] | min., R460 |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminium | 28.0 - 30.0 % Show Supplier Material materials with Aluminium of 28.0 - 30.0 % | Al₂O₃ |
Natrium | 17.0 - 19.0 % Show Supplier Material materials with Natrium of 17.0 - 19.0 % | Na₂O |
Silizium | 31.0 - 34.0 % Show Supplier Material materials with Silizium of 31.0 - 34.0 % | SiO₂ |
Technological properties
Property | ||
---|---|---|
Application areas | GNPGraystar’s Zeolites are used in multiple applications such as detergents, PVC stabilizers, brake pads, water treatment, construction (concrete/ asphalt), agricultre, adsorbents in pharmaceutical & food packaging, manufacture of paints, coatings & paper, as an oder remvoal agent, and many, many more applications. | |
Color | White | |