Allgemein
Property | Value | Comment |
---|---|---|
Loss on Ignition | 0.5 % Show Supplier Material materials with Loss on Ignition of 0.5 % | max. |
Schüttdichte | 3.1 - 3.2 g/cm³ Show Supplier Material materials with Schüttdichte of 3.1 - 3.2 g/cm³ | ASTM C357 |
Water content | 0.12 % Show Supplier Material materials with Water content of 0.12 % | |
0.5 % Show Supplier Material materials with Water content of 0.5 % |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminium | 87.5 % Show Supplier Material materials with Aluminium of 87.5 % | min. Al₂O₃ |
Eisen | 1.75 Show Supplier Material materials with Eisen of 1.75 | max. Fe₂O₃ |
Silizium | 7.5 Show Supplier Material materials with Silizium of 7.5 | max. SiO₂ |
Titan | 3.5 Show Supplier Material materials with Titan of 3.5 | max. TiO₂ |
Technological properties
Property | ||
---|---|---|
Other | See picture part of the datasheet for available sizing |