Chemical properties
Property | Value | Comment |
---|---|---|
Aluminium | 0.1 Show Supplier Material materials with Aluminium of 0.1 | max. Al₂O₃ |
Eisen | 0.1 Show Supplier Material materials with Eisen of 0.1 | max. Fe₂O₃ |
Kalzium | 0.1 % Show Supplier Material materials with Kalzium of 0.1 % | CaO |
Silizium | 0.4 Show Supplier Material materials with Silizium of 0.4 | max. SiO₂ |
Titan | 0.1 Show Supplier Material materials with Titan of 0.1 | max. TiO₂ |
Yttrium | 7.0 - 8.0 % Show Supplier Material materials with Yttrium of 7.0 - 8.0 % | Y₂O₃ |
Zirkonium | 90 % Show Supplier Material materials with Zirkonium of 90 % | ZrO₂ |
Technological properties
Property | ||
---|---|---|
Application areas | GNPGraystar’s Fused Yttria-Stabilized Zirconia is used for refractories, thermal spray coatings, plasma spraying, oxygen permeable membranes, ceramic rings, and many other applications. | |
Color | Yellow | |
Other | Custom Sizing available |