Allgemein
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminium | 0.4 Show Supplier Material materials with Aluminium of 0.4 | max. Al₂O₃ |
Eisen | 0.1 Show Supplier Material materials with Eisen of 0.1 | max. Fe₂O₃ |
Magnesium | 3.0 - 4.0 % Show Supplier Material materials with Magnesium of 3.0 - 4.0 % | MgO |
Silizium | 0.4 Show Supplier Material materials with Silizium of 0.4 | max. SiO₂ |
Titan | 0.2 Show Supplier Material materials with Titan of 0.2 | max. TiO₂ |
Zirkonium | 94 % Show Supplier Material materials with Zirkonium of 94 % | min. ZrO₂ |
Technological properties
Property | ||
---|---|---|
Application areas | GNPGraystar’s Fused MagnesiaStabilized Zirconia is used in various ceramic applications such as refractory setters for the electro-ceramic industry, zirconia furnace furniture, structural ceramics, sizing nozzles, and more. | |
Color | Yellow | |
Other | Custom Sizing available |