Allgemein
Property | Value | Comment |
---|---|---|
Partikelgrößenbereich | 3.0 - 6.0 µm Show Supplier Material materials with Partikelgrößenbereich of 3.0 - 6.0 µm | |
Spezifische Oberfläche | 10.0 Show Supplier Material materials with Spezifische Oberfläche of 10.0 | max. |
Chemical properties
Property | Value | Comment |
---|---|---|
Eisen | 0.003 Show Supplier Material materials with Eisen of 0.003 | max. Fe₂O₃ |
Natrium | 0.003 Show Supplier Material materials with Natrium of 0.003 | max. Na₂O |
Silizium | 0.015 Show Supplier Material materials with Silizium of 0.015 | max. SiO₂ |
Titan | 0.003 Show Supplier Material materials with Titan of 0.003 | max. TiO₂ |
Zirkonium | 99.9 % Show Supplier Material materials with Zirkonium of 99.9 % | ZrO₂+HfO₂ |
Technological properties
Property | ||
---|---|---|
Application areas | GNPGraystar’s Chemical Grade Monoclinic Zirconia is used in precision ceramics, electrical components, glass additives, ceramic colored glazes, refractory materials, polishing applications, and synthetic jewelry | |
Color | White | |
Other | SSA & Particle Size can be customized |