Allgemein
Chemical properties
Property | Value | Comment |
---|---|---|
Eisen | 0.002 Show Supplier Material materials with Eisen of 0.002 | max. Fe₂O₃ |
Silizium | 0.02 Show Supplier Material materials with Silizium of 0.02 | max. SiO₂ |
Titan | 0.002 Show Supplier Material materials with Titan of 0.002 | max. TiO₂ |
Zirkonium | 99.5 % Show Supplier Material materials with Zirkonium of 99.5 % | ZrO₂+HfO₂ |
Technological properties
Property | ||
---|---|---|
Application areas | GNPGraystar’s Chemical Grade Monoclinic Zirconia is used in precision ceramics, electrical components, glass additives, ceramic colored glazes, refractory materials, polishing applications, and synthetic jewelry | |
Color | White | |
Other | SSA & Particle Size can be customized |