Allgemein
Property | Value | Comment |
---|---|---|
Loss on Ignition | 1 % Show Supplier Material materials with Loss on Ignition of 1 % | |
Partikelgröße D50 | 0.8 Show Supplier Material materials with Partikelgröße D50 of 0.8 | max. |
Spezifische Oberfläche | 5.0 - 20.0 m²/g Show Supplier Material materials with Spezifische Oberfläche of 5.0 - 20.0 m²/g |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminium | 0.21 - 0.25 % Show Supplier Material materials with Aluminium of 0.21 - 0.25 % | Al₂O₃ |
Eisen | 0.003 Show Supplier Material materials with Eisen of 0.003 | max. Fe₂O₃ |
Natrium | 0.005 Show Supplier Material materials with Natrium of 0.005 | max. Na₂O |
Silizium | 0.02 Show Supplier Material materials with Silizium of 0.02 | max. SiO₂ |
Titan | 0.002 Show Supplier Material materials with Titan of 0.002 | max. TiO₂ |
Yttrium | 5.0 - 5.5 % Show Supplier Material materials with Yttrium of 5.0 - 5.5 % | Y₂O₃ |
Zirkonium | 94 % Show Supplier Material materials with Zirkonium of 94 % | ZrO₂+HfO₂ |
Technological properties
Property | ||
---|---|---|
Application areas | GNPGraystar’s Chemical Grade Yttria Stabilized Zirconia is used in various ceramic applications where high strength and resistance to wear is necessary. Examples include electrical ceramics, bioceramics, advanced refractory materials, optical fiber components, mechnical parts, cutting tools, oxygen sensors, solid oxide fuel cells, etc. | |
Color | White | |
Other | SSA & Particle Size can be customized |