Allgemein
Chemical properties
Property | Value | Comment |
---|---|---|
Eisen | 0.003 Show Supplier Material materials with Eisen of 0.003 | max. Fe₂O₃ |
Natrium | 0.005 Show Supplier Material materials with Natrium of 0.005 | max. Na₂O |
Silizium | 0.05 Show Supplier Material materials with Silizium of 0.05 | max. SiO₂ |
Titan | 0.002 Show Supplier Material materials with Titan of 0.002 | max. TiO₂ |
Yttrium | 13.25 - 13.75 % Show Supplier Material materials with Yttrium of 13.25 - 13.75 % | Y₂O₃ |
Zirkonium | 86 % Show Supplier Material materials with Zirkonium of 86 % | ZrO₂+HfO₂ |
Technological properties
Property | ||
---|---|---|
Application areas | GNPGraystar’s Chemical Grade Yttria Stabilized Zirconia is used in various ceramic applications where high strength and resistance to wear is necessary. Examples include electrical ceramics, bioceramics, advanced refractory materials, optical fiber components, mechnical parts, cutting tools, oxygen sensors, solid oxide fuel cells, etc. | |
Color | White |