Allgemein
Property | Value | Comment |
---|---|---|
Loss on Ignition | 1.5 % Show Supplier Material materials with Loss on Ignition of 1.5 % | Resistance Furnace |
3 % Show Supplier Material materials with Loss on Ignition of 3 % | Resistance Furnace | |
Schüttdichte | 1.25 - 1.45 g/cm³ Show Supplier Material materials with Schüttdichte of 1.25 - 1.45 g/cm³ | Hall Meter |
Spezifische Oberfläche | 5.0 - 20.0 m²/g Show Supplier Material materials with Spezifische Oberfläche of 5.0 - 20.0 m²/g | BET |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminium | 0.05 Show Supplier Material materials with Aluminium of 0.05 | max. Al₂O₃ unsing SICP | |
Eisen | 0.0025 Show Supplier Material materials with Eisen of 0.0025 | max.Fe₂O₃ using ICP | |
Magnesium | 3.4 - 3.6 % Show Supplier Material materials with Magnesium of 3.4 - 3.6 % | MgO using ICP | |
Silizium | 0.02 Show Supplier Material materials with Silizium of 0.02 | max. SiO₂ using ICP | |
Titan | 0.0025@max. TiO₂ using ICP | ||
Zirkonium | 96.2 - 96.6 % Show Supplier Material materials with Zirkonium of 96.2 - 96.6 % | ZrO₂+HfO₂ using XRF |
Technological properties
Property | ||
---|---|---|
Application areas | GNPGraystar’s Chemical Grade Magnesia-Stabilized Zirconia is an ideal material for valve and pump components, bushings and wear sleeves, industrial tool applications, as well as oil and gas down-hole tools. | |
Color | White, Yellow |