Allgemein
Property | Value | Comment |
---|---|---|
Loss on Ignition | 0.17 % Show Supplier Material materials with Loss on Ignition of 0.17 % | Resistance Furnace |
Schüttdichte | 1.13 g/cm³ Show Supplier Material materials with Schüttdichte of 1.13 g/cm³ | MS2000 Size Analyzer |
Spezifische Oberfläche | 4.0 m²/g Show Supplier Material materials with Spezifische Oberfläche of 4.0 m²/g | SSA-3600 BET |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminium | 0.001 Show Supplier Material materials with Aluminium of 0.001 | max. Al₂O₃ using pectrophotometry | |
Eisen | 0.003 Show Supplier Material materials with Eisen of 0.003 | max. Fe₂O₃ using spectrophotometry | |
Magnesium | 2.5 - 2.9 % Show Supplier Material materials with Magnesium of 2.5 - 2.9 % | MgO spectrophotometry | |
Silizium | 0.007 Show Supplier Material materials with Silizium of 0.007 | max. SiO₂ using spectrophotometry | |
Titan | 0.001@max. TiO₂ using spectrophotometry | ||
Zirkonium | 94.6 - 94.8 % Show Supplier Material materials with Zirkonium of 94.6 - 94.8 % | ZrO₂+HfO₂ using Bitter Almond Acid Gravimetric Method |
Technological properties
Property | ||
---|---|---|
Application areas | GNPGraystar’s Chemical Grade Magnesia-Stabilized Zirconia is an ideal material for valve and pump components, bushings and wear sleeves, industrial tool applications, as well as oil and gas down-hole tools. | |
Color | White |