Allgemein
Property | Value | Comment |
---|---|---|
Kristallgröße | 12.0 μm Show Supplier Material materials with Kristallgröße of 12.0 μm | |
Schüttdichte | 2.02 - 2.34 g/cm³ Show Supplier Material materials with Schüttdichte of 2.02 - 2.34 g/cm³ | ANSI B74.4 |
True particle density | 4.6 g/cm³ Show Supplier Material materials with True particle density of 4.6 g/cm³ |
Mechanisch
Thermisch
Property | Value |
---|---|
Schmelzpunkt | 1900.0 °C Show Supplier Material materials with Schmelzpunkt of 1900.0 °C |
Chemical properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Aluminium | 60 % Show Supplier Material materials with Aluminium of 60 % | ANSI B74.14 | max. Al₂O₃ |
Eisen | 0.25 % Show Supplier Material materials with Eisen of 0.25 % | ANSI B74.14 | Fe₂O₃ |
Kalzium | 0.09 % Show Supplier Material materials with Kalzium of 0.09 % | ANSI B74.14 | CaO |
Magnesium | 0.02 % Show Supplier Material materials with Magnesium of 0.02 % | ANSI B74.14 | MgO |
Natrium | 0.03 % Show Supplier Material materials with Natrium of 0.03 % | ANSI B74.14 | Na₂O |
Silizium | 0.33 % Show Supplier Material materials with Silizium of 0.33 % | ANSI B74.14 | SiO₂ |
Titan | 0.25 % Show Supplier Material materials with Titan of 0.25 % | ANSI B74.14 | TiO₂ |
Zirkonium | 39 % Show Supplier Material materials with Zirkonium of 39 % | ANSI B74.14 | ZrO₂ |
Technological properties
Property | ||
---|---|---|
Application areas | GNPGraystar’s Alumina Zirconia 40% is used for both coated abrasive products and organic bonded grinding wheels. |