Allgemein
Property | Value |
---|---|
Dichte | 3.16 g/cm³ Show Supplier Material materials with Dichte of 3.16 g/cm³ |
Porosität | 6.0 % Show Supplier Material materials with Porosität of 6.0 % |
Thermisch
Property | Value |
---|---|
Max. Betriebstemperatur | 1700.0 °C Show Supplier Material materials with Max. Betriebstemperatur of 1700.0 °C |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminium | 75.0 - 77.0 % Show Supplier Material materials with Aluminium of 75.0 - 77.0 % | Al₂O₃ |
Eisen | 0.1 Show Supplier Material materials with Eisen of 0.1 | max. Fe₂O₃ |
Kalzium | 0.05 Show Supplier Material materials with Kalzium of 0.05 | max. CaO |
Natrium | 0.1 Show Supplier Material materials with Natrium of 0.1 | max. Na₂O |
Silizium | 22.5 - 24.5 % Show Supplier Material materials with Silizium of 22.5 - 24.5 % | SiO₂ |
Titan | 0.02 Show Supplier Material materials with Titan of 0.02 | max. TiO₂ |
Technological properties
Property | ||
---|---|---|
Application areas | GNPGraystar’s White Fused Mullite is used in the investment casting, for producing refractories for the steel industry for the production of high purity mullite blocks for glass melting furnaces, for kiln furniture, and many other applications. | |
Crystal structure | Mullite Phase: 93%, α - Al2O3 Phase: 3%, Glassy Phase: 4% | |
Other | Available sizing: 3-5 mm, 1-3mm, 0.5-1 mm, 0-1 mm, 0-0.5 mm, 0-0.1 mm, 200/F, 325 F Other sizes are available upon request. |