Thermisch
Property | Value |
---|---|
Max. Betriebstemperatur | 1750.0 °C Show Supplier Material materials with Max. Betriebstemperatur of 1750.0 °C |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminium | 44.5 - 47.0 % Show Supplier Material materials with Aluminium of 44.5 - 47.0 % | Al₂O₃ |
Eisen | 0.2 Show Supplier Material materials with Eisen of 0.2 | max. Fe₂O₃ |
Natrium | 0.25 Show Supplier Material materials with Natrium of 0.25 | max. Na₂O |
Silizium | 16.0 - 18.0 % Show Supplier Material materials with Silizium of 16.0 - 18.0 % | SiO₂ |
Titan | 0.18 Show Supplier Material materials with Titan of 0.18 | max. TiO₂ |
Zirkonium | 34.0 - 38.5 % Show Supplier Material materials with Zirkonium of 34.0 - 38.5 % | ZrO₂ |
Technological properties
Property | ||
---|---|---|
Application areas | GNPGraystar’s Fused Zirconia Mullite is an excellent material for refractory applications such as glide gates, nozzles, and special refractory parts for the glass industry. | |
Crystal structure | α - Al2O3 Phase: 4% | |
Other | Available sizing: 3-5 mm, 1-3mm, 0.5-1 mm, 0-1 mm, 0-0.5 mm, 0-0.1 mm, 200/F, 325/F Other sizes are available upon request. |