Allgemein
Property | Value |
---|---|
True particle density | 5.05 g/cm³ Show Supplier Material materials with True particle density of 5.05 g/cm³ |
Thermisch
Property | Value |
---|---|
Schmelzpunkt | 2410.0 °C Show Supplier Material materials with Schmelzpunkt of 2410.0 °C |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminium | 0.01 Show Supplier Material materials with Aluminium of 0.01 | max. Al₂O₃ |
Eisen | 0.01 Show Supplier Material materials with Eisen of 0.01 | max. Fe₂O₃ |
Silizium | 0.02 Show Supplier Material materials with Silizium of 0.02 | max. SiO₂ |
Titan | 0.01 Show Supplier Material materials with Titan of 0.01 | max. TiO₂ |
Yttrium | 99.5 % Show Supplier Material materials with Yttrium of 99.5 % | min. Y₂O₃ |
Technological properties
Property | ||
---|---|---|
Application areas | GNPGraystar’s Fused Yttrium Oxide is typically used in the titanium casting and specialty ceramics industries. | |
Other | Available Sizing: |