Allgemein
Property | Value | Comment |
---|---|---|
Loss on Ignition | 1 % Show Supplier Material materials with Loss on Ignition of 1 % | max., (1000°C/2 hrs) |
Partikelgröße D50 | 2.0 - 10.0 μm Show Supplier Material materials with Partikelgröße D50 of 2.0 - 10.0 μm | PSD |
Spezifische Oberfläche | 2.0 - 12.0 m²/g Show Supplier Material materials with Spezifische Oberfläche of 2.0 - 12.0 m²/g |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminium | 0.025 Show Supplier Material materials with Aluminium of 0.025 | max. Al₂O₃ |
Andere | 0.1 Show Supplier Material materials with Andere of 0.1 | Total Remaining RE-Oxides |
Eisen | 0.005 Show Supplier Material materials with Eisen of 0.005 | max. Fe₂O₃ |
Kalium | 0.006 Show Supplier Material materials with Kalium of 0.006 | max. K₂O |
Kalzium | 0.006 Show Supplier Material materials with Kalzium of 0.006 | max. CaO |
Natrium | 0.006 Show Supplier Material materials with Natrium of 0.006 | max. Na₂O |
Silizium | 0.05 Show Supplier Material materials with Silizium of 0.05 | max. SiO₂ |
Yttrium | 99.9 % Show Supplier Material materials with Yttrium of 99.9 % | min. Y₂O₃ |
Technological properties
Property | ||
---|---|---|
Application areas | It is typically used in the manufacturing of mono and polycrystalline ferrite materials in the electronic industry, for the synthesis of gemstones, as a glass additive to increase the refractive index and reduce light dispersion in glass, such as camera lenses, for optical systems and lenses for extreme temperatures, for refractory and conductive ceramics, oxygen sensors for emission control, for the production of ceramic pigments, as well as pole impregnation in batteries, lasers, and accumulators. |