Allgemein
Property | Value | Comment |
---|---|---|
Loss on Ignition | 0.1 % Show Supplier Material materials with Loss on Ignition of 0.1 % | max. |
Partikelgröße D50 | 1.0 - 40.0 μm Show Supplier Material materials with Partikelgröße D50 of 1.0 - 40.0 μm | different specifications, please refer to the table below |
True particle density | 2.15 g/cm³ Show Supplier Material materials with True particle density of 2.15 g/cm³ | |
2.25 g/cm³ Show Supplier Material materials with True particle density of 2.25 g/cm³ |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminium | 0.15 Show Supplier Material materials with Aluminium of 0.15 | max. Al₂O₃ |
Chlor | 0.0005 Show Supplier Material materials with Chlor of 0.0005 | max. Cl⁻ |
Eisen | 0.0015 Show Supplier Material materials with Eisen of 0.0015 | Fe²⁺ |
0.01 Show Supplier Material materials with Eisen of 0.01 | max. Fe₂O₃ | |
Kalium | 0.008 Show Supplier Material materials with Kalium of 0.008 | max. K₂O |
Kalzium | 0.008 Show Supplier Material materials with Kalzium of 0.008 | max. CaO |
Magnesium | 0.008 Show Supplier Material materials with Magnesium of 0.008 | |
Natrium | 0.0005 Show Supplier Material materials with Natrium of 0.0005 | Na⁺ |
0.01 Show Supplier Material materials with Natrium of 0.01 | max. Na₂O | |
Silizium | 99.3 % Show Supplier Material materials with Silizium of 99.3 % | min. SiO₂ |
Titan | 0.008 Show Supplier Material materials with Titan of 0.008 | max. TiO₂ |
Technological properties
Property | ||
---|---|---|
Application areas | GNPGraystar’s Spherical Fused Silica Powder is widely used in various industries such as encapsulation of electronic products and chip material, fiber optic cable, special engineering plastics, rubber, cermic, filler for heat dissipation board (MC board), heat dissipating grease, ink, chemical industry, and many other applications. | |
Other |