Allgemein
Mechanisch
Property | Value |
---|---|
Härte, Mohs | 9.0 [-] Show Supplier Material materials with Härte, Mohs of 9.0 [-] |
Technological properties
Property | ||
---|---|---|
Application areas | GNPGraystar’s Alumin Grinding Media is used in wet grinding (batch and continuous ball mills), ceramic glaze grinding, and in dry grinding of resins, ceramic raw materials, and other mineral products. | |
Other | Beads/Balls are available in 1, 3, 6, 8, 10, 13, 15, 18, 20, 25, 30, 35, 40, 45, 50, 60, 70, & 80 mm diamters. Cylinders are available in 12x12, 20x20, 30x30, 35x35, 40x45, and 50x55 mm. Other sizes/shapes available upon request. | |
Wear resistance | Wear rate of maximum 0.15% |