Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 5.95 - 6.0 g/cm³ Show Supplier Material materials with Dichte of 5.95 - 6.0 g/cm³ | packed density: 3.6-3.8 |
Wasserabsorption | 0 % Show Supplier Material materials with Wasserabsorption of 0 % |
Mechanisch
Chemical properties
Property | Value | Comment |
---|---|---|
Zirkonium | 95 % Show Supplier Material materials with Zirkonium of 95 % | ZrO₂+CeO₂ |
Technological properties
Property | ||
---|---|---|
Application areas | GNPGraystar’s Zirconia Grinding Media is used for audio/video recording tapes, electronic-grade ceramics, ferroelectric, piezoelectric, dielectric, capacitors, sensors, inks, dyes, paint, and other pigments. | |
Color | Gold | |
Other | Available Sizes: Ceria Stabilized Spheres: Φ0.4, Φ0.5, Φ0.8, Φ1, Φ1.5, Φ2, Φ2.5, Φ3, Φ4, Φ5, Φ7, Φ8, Φ10, Φ12, Φ15, Φ20, Φ25, Φ30 mm | |
Wear resistance | Wear Rate (normal): <0.3% , (extreme): <2% |