Chemical properties
Property | Value | Comment |
---|---|---|
Aluminium | 97.5 % Show Supplier Material materials with Aluminium of 97.5 % | Al₂O₃ |
Chrom | 1.9 % Show Supplier Material materials with Chrom of 1.9 % | Cr₂O₃ |
Eisen | 0.07 % Show Supplier Material materials with Eisen of 0.07 % | Fe₂O₃ |
Natrium | 0.3 % Show Supplier Material materials with Natrium of 0.3 % | Na₂O |
Technological properties
Property | ||
---|---|---|
Application areas | The FEPA F grades are especially suitable for the manufacture of vitrified bonded abrasives for working hardened steels and alloys with tensile strengths of over 50 kg/ mm2. These are also used in tool grinding, saw and knife-sharpening applications, precision grinding, profile grinding, flute grinding, tooth grinding, dry grinding of blade segments, and mounted wheels. | |
Color | Ruby | |
Other |