Allgemein
Property | Value | Comment |
---|---|---|
Partikelgrößenbereich | 2000.0 µm Show Supplier Material materials with Partikelgrößenbereich of 2000.0 µm | |
Schüttdichte | 0.65 - 1.1 g/cm³ Show Supplier Material materials with Schüttdichte of 0.65 - 1.1 g/cm³ | depending on the size, refer to the table below |
Thermisch
Property | Value |
---|---|
Schmelzpunkt | 2100.0 °C Show Supplier Material materials with Schmelzpunkt of 2100.0 °C |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminium | 98.8 % Show Supplier Material materials with Aluminium of 98.8 % | Al₂O₃ |
Eisen | 0.04 Show Supplier Material materials with Eisen of 0.04 | Fe₂O₃ |
Kalzium | 0.03 Show Supplier Material materials with Kalzium of 0.03 | CaO |
Magnesium | 0.08 Show Supplier Material materials with Magnesium of 0.08 | |
Natrium | 0.09 Show Supplier Material materials with Natrium of 0.09 | Na₂O |
Silizium | 0.8 Show Supplier Material materials with Silizium of 0.8 | SiO₂ |
Technological properties
Property | ||
---|---|---|
Application areas | Due to the above noted properties, Bubble Alumina is used in lightweight, high temperature refractories to form pores in high-porosity abrasives, and as a media to filtrate aggressive liquids or melts. It can also be used as a bed materials in the firing process of vitirified grinding wheels and other ceramic parts. | |
Color | White | |
Crystal structure | Alpha-Alumina | |
Other | Available Sizes & Typical Bulk Densities: |