Property | Value |
---|---|
Dichte | 2.4 - 2.6 g/cm³ Show Supplier Material materials with Dichte of 2.4 - 2.6 g/cm³ |
Schüttdichte | 1.4 - 1.6 g/cm³ Show Supplier Material materials with Schüttdichte of 1.4 - 1.6 g/cm³ |
Mechanisch
Property | Value |
---|---|
Härte, Knoop, HK2 | 600 [-] Show Supplier Material materials with Härte, Knoop, HK2 of 600 [-] |
Technological properties
Property | ||
---|---|---|
Certifications | RockRidge Glass Beads meet all Occupational Health and Safety Administration (OSHA) requirements. RockRidge Glass Beads do not contain free-silica and meet all ISO 11126-10:200 requirements. | |