Allgemein
Property | Value | Comment |
---|---|---|
Loss on Ignition | 1 % Show Supplier Material materials with Loss on Ignition of 1 % | max. (1000°C/2 hrs) |
Partikelgröße D50 | 2.0 - 10.0 μm Show Supplier Material materials with Partikelgröße D50 of 2.0 - 10.0 μm | PSD |
Chemical properties
Property | Value | Comment |
---|---|---|
Andere | 0.01 Show Supplier Material materials with Andere of 0.01 | Total Remaining RE-Oxides |
Eisen | 0.001 Show Supplier Material materials with Eisen of 0.001 | max. Fe₂O₃ |
Kalzium | 0.01 Show Supplier Material materials with Kalzium of 0.01 | max. CaO |
Kobalt | 0.0002 % Show Supplier Material materials with Kobalt of 0.0002 % | max. Co₃O₄ |
Nickel | 0.0002 Show Supplier Material materials with Nickel of 0.0002 | max. NiO |
Silizium | 0.01 Show Supplier Material materials with Silizium of 0.01 | |
Ytterbium | 99.99 % Show Supplier Material materials with Ytterbium of 99.99 % | min. Yb₂O₃ |
Technological properties
Property | ||
---|---|---|
Application areas | It is typically used as a phosphor activator and in coding material for security systems. |