Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 14.49 g/cm³ Show Supplier Material materials with Dichte of 14.49 g/cm³ | |
Korngröße | 6 - 10 μm Show Supplier Material materials with Korngröße of 6 - 10 μm | tungsten carbide grain size | |
Partikelgröße D90 | 25 μm Show Supplier Material materials with Partikelgröße D90 of 25 μm | max |
Mechanisch
Property | Temperature | Value |
---|---|---|
Härte, Vickers, 30 | 23.0 °C | 1100 [-] Show Supplier Material materials with Härte, Vickers, 30 of 1100 [-] |
Magnetisch
Property | Temperature | Value |
---|---|---|
Koerzitivfeldstärke | 23.0 °C | 5174 A/m Show Supplier Material materials with Koerzitivfeldstärke of 5174 A/m |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminium | 0.02 % Show Supplier Material materials with Aluminium of 0.02 % | max | |
Andere | 0.2 % Show Supplier Material materials with Andere of 0.2 % | Ti+Ta+Nb | |
Chrom | 0.05 % Show Supplier Material materials with Chrom of 0.05 % | max | |
Eisen | 0.3 % Show Supplier Material materials with Eisen of 0.3 % | max | |
Kobalt | 5 - 8 % Show Supplier Material materials with Kobalt of 5 - 8 % | ||
Kohlenstoff | as WC balance | ||
Kupfer | 0.02 % Show Supplier Material materials with Kupfer of 0.02 % | max | |
Nickel | 0.1 % Show Supplier Material materials with Nickel of 0.1 % | max | |
Sauerstoff | 0.3 % Show Supplier Material materials with Sauerstoff of 0.3 % | max | |
Vanadium | 0.01 % Show Supplier Material materials with Vanadium of 0.01 % | max | |
Wolfram | as WC balance | ||
Zink | 5E-3 % Show Supplier Material materials with Zink of 5E-3 % | max |
Technological properties
Property | ||
---|---|---|
Application areas | Powder Grade EC with it’s low cobalt content and extra coarse, very uniform WC grain size distribution is the perfect powder for multiple mining and rock drilling applications. This material requires only short milling in the ready-to-press powder production and offers good sintered properties. |