Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 14.49 g/cm³ Show Supplier Material materials with Dichte of 14.49 g/cm³ | |
Korngröße | 0.8 - 1.3 μm Show Supplier Material materials with Korngröße of 0.8 - 1.3 μm | tungsten carbide grain size | |
Partikelgröße D90 | 6 μm Show Supplier Material materials with Partikelgröße D90 of 6 μm | max |
Mechanisch
Property | Temperature | Value |
---|---|---|
Härte, Vickers, 30 | 23.0 °C | 1600 [-] Show Supplier Material materials with Härte, Vickers, 30 of 1600 [-] |
Magnetisch
Property | Temperature | Value |
---|---|---|
Koerzitivfeldstärke | 23.0 °C | 20696 A/m Show Supplier Material materials with Koerzitivfeldstärke of 20696 A/m |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminium | 0.02 % Show Supplier Material materials with Aluminium of 0.02 % | max | |
Chrom | 0.6 % Show Supplier Material materials with Chrom of 0.6 % | max | |
Eisen | 0.3 % Show Supplier Material materials with Eisen of 0.3 % | max | |
Kobalt | 8 - 12 % Show Supplier Material materials with Kobalt of 8 - 12 % | ||
Kohlenstoff | as WC balance | ||
Kupfer | 0.02 % Show Supplier Material materials with Kupfer of 0.02 % | max | |
Nickel | 0.1 % Show Supplier Material materials with Nickel of 0.1 % | max | |
Niobium | 0.1 % Show Supplier Material materials with Niobium of 0.1 % | max | |
Sauerstoff | 0.5 % Show Supplier Material materials with Sauerstoff of 0.5 % | max | |
Tantal | 0.1 % Show Supplier Material materials with Tantal of 0.1 % | max | |
Titan | 0.1 % Show Supplier Material materials with Titan of 0.1 % | max | |
Vanadium | 0.2 % Show Supplier Material materials with Vanadium of 0.2 % | max | |
Wolfram | as WC balance | ||
Zink | 5E-3 % Show Supplier Material materials with Zink of 5E-3 % | max |
Technological properties
Property | ||
---|---|---|
Application areas | Powder grade F Premium was developed for use in a wide range of tooling products, such as hardmetal rods, indexable inserts, woodworking tools and wear parts. | |
Other | Extremely fine particle sized powder with submicron WC grain size is the optimum solution to applications like extrusion of hard metal rods, knives and others where coarse WC grains are not allowed. When comparing to standard grade F powder, F Premium has a higher shrinkage rate. |