Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 14.49 g/cm³ Show Supplier Material materials with Dichte of 14.49 g/cm³ | |
Korngröße | 0.8 - 1.3 μm Show Supplier Material materials with Korngröße of 0.8 - 1.3 μm | tungsten carbide grain size | |
Partikelgröße D90 | 16 μm Show Supplier Material materials with Partikelgröße D90 of 16 μm | max |
Mechanisch
Property | Temperature | Value |
---|---|---|
Härte, Vickers, 30 | 23.0 °C | 1560 [-] Show Supplier Material materials with Härte, Vickers, 30 of 1560 [-] |
Magnetisch
Property | Temperature | Value |
---|---|---|
Koerzitivfeldstärke | 23.0 °C | 19104 A/m Show Supplier Material materials with Koerzitivfeldstärke of 19104 A/m |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminium | 0.02 % Show Supplier Material materials with Aluminium of 0.02 % | max | |
Chrom | 0.6 % Show Supplier Material materials with Chrom of 0.6 % | max | |
Eisen | 0.3 % Show Supplier Material materials with Eisen of 0.3 % | max | |
Kobalt | 8 - 12 % Show Supplier Material materials with Kobalt of 8 - 12 % | ||
Kohlenstoff | as WC balance | ||
Kupfer | 0.02 % Show Supplier Material materials with Kupfer of 0.02 % | max | |
Nickel | 0.1 % Show Supplier Material materials with Nickel of 0.1 % | max | |
Niobium | 0.1 % Show Supplier Material materials with Niobium of 0.1 % | max | |
Sauerstoff | 0.3 % Show Supplier Material materials with Sauerstoff of 0.3 % | max | |
Tantal | 0.1 % Show Supplier Material materials with Tantal of 0.1 % | max | |
Titan | 0.1 % Show Supplier Material materials with Titan of 0.1 % | max | |
Vanadium | 0.2 % Show Supplier Material materials with Vanadium of 0.2 % | max | |
Wolfram | as WC balance | ||
Zink | 5E-3 % Show Supplier Material materials with Zink of 5E-3 % | max |
Technological properties
Property | ||
---|---|---|
Application areas | Powder grade F was developed for use in a wide range of tooling products, such as hardmetal rods, indexable inserts, woodworking tools and wear parts. | |
Other | Grade F powder exhibits a unifrom WC grain size distribution with evenly distributed WC and Cobalt particles. Thanks to the fine particle size of the powder, milling characteristics are great and comparable to virgin WC-Co powders. |