Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 14.49 g/cm³ Show Supplier Material materials with Dichte of 14.49 g/cm³ | |
Korngröße | 1.3 - 3.5 μm Show Supplier Material materials with Korngröße of 1.3 - 3.5 μm | tungsten carbide grain size | |
Partikelgröße D90 | 16 μm Show Supplier Material materials with Partikelgröße D90 of 16 μm | max |
Mechanisch
Property | Temperature | Value |
---|---|---|
Härte, Vickers, 30 | 23.0 °C | 1360 [-] Show Supplier Material materials with Härte, Vickers, 30 of 1360 [-] |
Magnetisch
Property | Temperature | Value |
---|---|---|
Koerzitivfeldstärke | 23.0 °C | 9552 A/m Show Supplier Material materials with Koerzitivfeldstärke of 9552 A/m |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminium | 0.02 % Show Supplier Material materials with Aluminium of 0.02 % | max | |
Andere | 0.5 % Show Supplier Material materials with Andere of 0.5 % | Ti+Ta+Nb | |
Chrom | 0.2 % Show Supplier Material materials with Chrom of 0.2 % | max | |
Eisen | 0.6 % Show Supplier Material materials with Eisen of 0.6 % | max | |
Kobalt | 6 - 20 % Show Supplier Material materials with Kobalt of 6 - 20 % | ||
Kohlenstoff | as WC balance | ||
Kupfer | 0.02 % Show Supplier Material materials with Kupfer of 0.02 % | max | |
Nickel | 0.15 % Show Supplier Material materials with Nickel of 0.15 % | max | |
Sauerstoff | 0.3 % Show Supplier Material materials with Sauerstoff of 0.3 % | max | |
Vanadium | 0.1 % Show Supplier Material materials with Vanadium of 0.1 % | max | |
Wolfram | as WC balance | ||
Zink | 5E-3 % Show Supplier Material materials with Zink of 5E-3 % | max |
Technological properties
Property | ||
---|---|---|
Application areas | Powder grade M was developed for use in a wide range of tooling products, such as indexable inserts, woodworking tools and wear parts. | |
Other | Powder Grade M has evenly distributed WC and Cobalt particles with a fine particle size. Thanks to excellent milling characteristics, the same powder processing parameters can be utilized with Grade M as used with virgin WC-Co powders. |