Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 13.24 g/cm³ Show Supplier Material materials with Dichte of 13.24 g/cm³ | |
Korngröße | 1.3 - 3.5 μm Show Supplier Material materials with Korngröße of 1.3 - 3.5 μm | tungsten carbide grain size | |
Partikelgröße D90 | 16 μm Show Supplier Material materials with Partikelgröße D90 of 16 μm | max |
Mechanisch
Property | Temperature | Value |
---|---|---|
Härte, Vickers, 30 | 23.0 °C | 1145 [-] Show Supplier Material materials with Härte, Vickers, 30 of 1145 [-] |
Magnetisch
Property | Temperature | Value |
---|---|---|
Koerzitivfeldstärke | 23.0 °C | 10188 A/m Show Supplier Material materials with Koerzitivfeldstärke of 10188 A/m |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminium | 0.05 % Show Supplier Material materials with Aluminium of 0.05 % | max | |
Chrom | 0.2 % Show Supplier Material materials with Chrom of 0.2 % | max | |
Eisen | 0.5 % Show Supplier Material materials with Eisen of 0.5 % | max | |
Kobalt | 7 - 12 % Show Supplier Material materials with Kobalt of 7 - 12 % | ||
Kohlenstoff | as WC balance | ||
Kupfer | 0.05 % Show Supplier Material materials with Kupfer of 0.05 % | max | |
Nickel | 0.5 % Show Supplier Material materials with Nickel of 0.5 % | max | |
Niobium | 0.3 % Show Supplier Material materials with Niobium of 0.3 % | max | |
Sauerstoff | 0.3 % Show Supplier Material materials with Sauerstoff of 0.3 % | max | |
Tantal | 0.7 % Show Supplier Material materials with Tantal of 0.7 % | max | |
Titan | 0.5 % Show Supplier Material materials with Titan of 0.5 % | max | |
Vanadium | 0.07 % Show Supplier Material materials with Vanadium of 0.07 % | max | |
Wolfram | as WC balance | ||
Zink | 5E-3 % Show Supplier Material materials with Zink of 5E-3 % | max |
Technological properties
Property | ||
---|---|---|
Application areas | Powder grade TS was developed for use in a wide range of tooling products, such as indexable inserts, woodworking tools and wear parts. | |
Other | Grade TS has a small amount of 1-2 μm sized cubic carbides which increases the hardness and decreases the density of the material. Thanks to the fine particle size of the powder, milling characteristics are great and comparable to virgin WC-Co powders. |