Abmessung
Property | Value |
---|---|
Dimensions | Rod: Diameter: up to 4.7 mm, Length: up to 2500 mm - Wire: Diameter: 0.2-1.6 mm ; various dimensions can be also customized |
Mechanisch
Thermisch
Property | Temperature | Value |
---|---|---|
Recrystallization temperature | 350 °C Show Supplier Material materials with Recrystallization temperature of 350 °C | |
Wärmeleitfähigkeit | 23.0 °C | 90.9 - 91 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 90.9 - 91 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
spezifischer Widerstand | 23.0 °C | 7.1E-8 Ω·m Show Supplier Material materials with spezifischer Widerstand of 7.1E-8 Ω·m |
Chemical properties
Technological properties
Property | ||
---|---|---|
Application areas | Wire: Sputter Targets, evaporation pellets, regulator coil in glow plugs of diesel engines; litz wire for current conduction under elevated temperatures and in aggressive environments, Pre material for thin wire manfacturing, Ni wire mesh, Thermal Spraying, Coating layer for corrosion protection from alkalis; salt spray; molten salt and reduciing chemicals; coating layer for high temperature resistance; corrosion protection at high temperatures; coating layer for membrane walls of power plants | |
Heat Treatment | Soft Annealed | |
Processing history | For producing wire, the 6 mm hot rolled thick plates are cut into 6 mm wide sticks. The sticks are frontally welded. Afterwards the raw wire can be treated in the same way as hot rolled wire produced by melt metallurgy. accordingly, the wire is drawn to the desired dimensions through cold drawing and intermediate annealing. | |
Surface Finish | Blank/Bare/bright surface |