Chemical properties
Property | Value |
---|---|
Aluminium | Balance |
Barium | 2E-6 % Show Supplier Material materials with Barium of 2E-6 % |
Blei | 5E-6 % Show Supplier Material materials with Blei of 5E-6 % |
Bor | 1.5E-5 % Show Supplier Material materials with Bor of 1.5E-5 % |
Chrom | 5E-6 % Show Supplier Material materials with Chrom of 5E-6 % |
Eisen | 5E-5 % Show Supplier Material materials with Eisen of 5E-5 % |
Gallium | 2E-6 % Show Supplier Material materials with Gallium of 2E-6 % |
Kalzium | 7E-6 % Show Supplier Material materials with Kalzium of 7E-6 % |
Magnesium | 5E-5 % Show Supplier Material materials with Magnesium of 5E-5 % |
Mangan | 5E-6 % Show Supplier Material materials with Mangan of 5E-6 % |
Nickel | 5E-6 % Show Supplier Material materials with Nickel of 5E-6 % |
Phosphor | 5E-5 % Show Supplier Material materials with Phosphor of 5E-5 % |
Silber | 5E-6 % Show Supplier Material materials with Silber of 5E-6 % |
Silizium | 5E-5 % Show Supplier Material materials with Silizium of 5E-5 % |
Titan | 1E-5 % Show Supplier Material materials with Titan of 1E-5 % |
Vanadium | 1E-5 % Show Supplier Material materials with Vanadium of 1E-5 % |
Zirkonium | 5E-6 % Show Supplier Material materials with Zirkonium of 5E-6 % |