Chemical properties
Property | Value |
---|---|
Aluminium | Balance |
Barium | 1E-5 % Show Supplier Material materials with Barium of 1E-5 % |
Blei | 1E-5 % Show Supplier Material materials with Blei of 1E-5 % |
Bor | 1E-5 % Show Supplier Material materials with Bor of 1E-5 % |
Chrom | 1E-5 % Show Supplier Material materials with Chrom of 1E-5 % |
Eisen | 2E-5 % Show Supplier Material materials with Eisen of 2E-5 % |
Gallium | 1E-5 % Show Supplier Material materials with Gallium of 1E-5 % |
Kalzium | 2E-5 % Show Supplier Material materials with Kalzium of 2E-5 % |
Magnesium | 2E-5 % Show Supplier Material materials with Magnesium of 2E-5 % |
Mangan | 1E-5 % Show Supplier Material materials with Mangan of 1E-5 % |
Natrium | 5E-5 % Show Supplier Material materials with Natrium of 5E-5 % |
Nickel | 1E-5 % Show Supplier Material materials with Nickel of 1E-5 % |
Phosphor | 5E-5 % Show Supplier Material materials with Phosphor of 5E-5 % |
Silber | 1E-5 % Show Supplier Material materials with Silber of 1E-5 % |
Silizium | 3E-5 % Show Supplier Material materials with Silizium of 3E-5 % |
Titan | 1E-5 % Show Supplier Material materials with Titan of 1E-5 % |
Vanadium | 2E-5 % Show Supplier Material materials with Vanadium of 2E-5 % |
Zink | 1E-5 % Show Supplier Material materials with Zink of 1E-5 % |
Zirkonium | 2E-5 % Show Supplier Material materials with Zirkonium of 2E-5 % |