Chemical properties
Property | Value |
---|---|
Aluminium | Balance |
Antimon | 8E-6 % Show Supplier Material materials with Antimon of 8E-6 % |
Arsen | 5E-6 % Show Supplier Material materials with Arsen of 5E-6 % |
Barium | 2E-6 % Show Supplier Material materials with Barium of 2E-6 % |
Beryllium | 1E-6 % Show Supplier Material materials with Beryllium of 1E-6 % |
Bismut | 5E-6 % Show Supplier Material materials with Bismut of 5E-6 % |
Blei | 5E-6 % Show Supplier Material materials with Blei of 5E-6 % |
Bor | 2E-6 % Show Supplier Material materials with Bor of 2E-6 % |
Caesium | 5E-6 % Show Supplier Material materials with Caesium of 5E-6 % |
Cerium | 1E-5 % Show Supplier Material materials with Cerium of 1E-5 % |
Chlor | 1E-5 % Show Supplier Material materials with Chlor of 1E-5 % |
Chrom | 4E-6 % Show Supplier Material materials with Chrom of 4E-6 % |
Eisen | 1E-5 % Show Supplier Material materials with Eisen of 1E-5 % |
Fluor | 1E-5 % Show Supplier Material materials with Fluor of 1E-5 % |
Gallium | 1E-6 % Show Supplier Material materials with Gallium of 1E-6 % |
Germanium | 1E-5 % Show Supplier Material materials with Germanium of 1E-5 % |
Indium | 5E-6 % Show Supplier Material materials with Indium of 5E-6 % |
Kalzium | 4E-6 % Show Supplier Material materials with Kalzium of 4E-6 % |
Kobalt | 1E-6 % Show Supplier Material materials with Kobalt of 1E-6 % |
Kupfer | 1E-5 % Show Supplier Material materials with Kupfer of 1E-5 % |
Lanthan | 6E-6 % Show Supplier Material materials with Lanthan of 6E-6 % |
Lithium | 1E-6 % Show Supplier Material materials with Lithium of 1E-6 % |
Magnesium | 1.5E-5 % Show Supplier Material materials with Magnesium of 1.5E-5 % |
Mangan | 2E-6 % Show Supplier Material materials with Mangan of 2E-6 % |
Molybdän | 2E-6 % Show Supplier Material materials with Molybdän of 2E-6 % |
Natrium | 5E-6 % Show Supplier Material materials with Natrium of 5E-6 % |
Nickel | 5E-6 % Show Supplier Material materials with Nickel of 5E-6 % |
Phosphor | 3E-5 % Show Supplier Material materials with Phosphor of 3E-5 % |
Platin | 1E-5 % Show Supplier Material materials with Platin of 1E-5 % |
Schwefel | 1E-5 % Show Supplier Material materials with Schwefel of 1E-5 % |
Silber | 5E-6 % Show Supplier Material materials with Silber of 5E-6 % |
Silizium | 1E-5 % Show Supplier Material materials with Silizium of 1E-5 % |
Thorium | 1E-6 % Show Supplier Material materials with Thorium of 1E-6 % |
Titan | 5E-6 % Show Supplier Material materials with Titan of 5E-6 % |
Uran | 1E-6 % Show Supplier Material materials with Uran of 1E-6 % |
Vanadium | 1E-5 % Show Supplier Material materials with Vanadium of 1E-5 % |
Wolfram | 5E-6 % Show Supplier Material materials with Wolfram of 5E-6 % |
Zink | 5E-6 % Show Supplier Material materials with Zink of 5E-6 % |
Zinn | 5E-6 % Show Supplier Material materials with Zinn of 5E-6 % |
Zirkonium | 3E-6 % Show Supplier Material materials with Zirkonium of 3E-6 % |