Chemical properties
Property | Value |
---|---|
Aluminium | Balance |
Antimon | 1E-6 % Show Supplier Material materials with Antimon of 1E-6 % |
Arsen | 1E-6 % Show Supplier Material materials with Arsen of 1E-6 % |
Barium | 2E-6 % Show Supplier Material materials with Barium of 2E-6 % |
Beryllium | 1E-6 % Show Supplier Material materials with Beryllium of 1E-6 % |
Bismut | 1E-6 % Show Supplier Material materials with Bismut of 1E-6 % |
Blei | 1E-6 % Show Supplier Material materials with Blei of 1E-6 % |
Bor | 2E-6 % Show Supplier Material materials with Bor of 2E-6 % |
Caesium | 1E-6 % Show Supplier Material materials with Caesium of 1E-6 % |
Cerium | 1E-6 % Show Supplier Material materials with Cerium of 1E-6 % |
Chlor | 1E-6 % Show Supplier Material materials with Chlor of 1E-6 % |
Chrom | 3E-6 % Show Supplier Material materials with Chrom of 3E-6 % |
Eisen | 7E-6 % Show Supplier Material materials with Eisen of 7E-6 % |
Fluor | 1E-6 % Show Supplier Material materials with Fluor of 1E-6 % |
Gallium | 1E-6 % Show Supplier Material materials with Gallium of 1E-6 % |
Germanium | 1E-6 % Show Supplier Material materials with Germanium of 1E-6 % |
Indium | 1E-6 % Show Supplier Material materials with Indium of 1E-6 % |
Kalzium | 2E-6 % Show Supplier Material materials with Kalzium of 2E-6 % |
Kobalt | 1E-6 % Show Supplier Material materials with Kobalt of 1E-6 % |
Kupfer | 8E-6 % Show Supplier Material materials with Kupfer of 8E-6 % |
Lanthan | 1E-6 % Show Supplier Material materials with Lanthan of 1E-6 % |
Lithium | 1E-6 % Show Supplier Material materials with Lithium of 1E-6 % |
Magnesium | 8E-6 % Show Supplier Material materials with Magnesium of 8E-6 % |
Mangan | 2E-6 % Show Supplier Material materials with Mangan of 2E-6 % |
Molybdän | 1E-6 % Show Supplier Material materials with Molybdän of 1E-6 % |
Natrium | 1E-6 % Show Supplier Material materials with Natrium of 1E-6 % |
Nickel | 1E-6 % Show Supplier Material materials with Nickel of 1E-6 % |
Phosphor | 1E-5 % Show Supplier Material materials with Phosphor of 1E-5 % |
Platin | 5E-6 % Show Supplier Material materials with Platin of 5E-6 % |
Schwefel | 5E-6 % Show Supplier Material materials with Schwefel of 5E-6 % |
Silber | 1E-6 % Show Supplier Material materials with Silber of 1E-6 % |
Silizium | 1E-5 % Show Supplier Material materials with Silizium of 1E-5 % |
Thorium | 1E-8 % Show Supplier Material materials with Thorium of 1E-8 % |
Titan | 4E-6 % Show Supplier Material materials with Titan of 4E-6 % |
Uran | 1E-8 % Show Supplier Material materials with Uran of 1E-8 % |
Vanadium | 4E-6 % Show Supplier Material materials with Vanadium of 4E-6 % |
Wolfram | 1E-6 % Show Supplier Material materials with Wolfram of 1E-6 % |
Zink | 1E-6 % Show Supplier Material materials with Zink of 1E-6 % |
Zinn | 1E-6 % Show Supplier Material materials with Zinn of 1E-6 % |
Zirkonium | 1E-6 % Show Supplier Material materials with Zirkonium of 1E-6 % |