Allgemein
Property | Value | Comment |
---|---|---|
Coefficient of friction | 0.34 [-] Show Supplier Material materials with Coefficient of friction of 0.34 [-] | DIN 53375, C, Against dry running steel |
Dichte | 1.78 g/cm³ Show Supplier Material materials with Dichte of 1.78 g/cm³ | ISO 1183 |
Wasserabsorption | 0.04 % Show Supplier Material materials with Wasserabsorption of 0.04 % | max., ISO 62 |
Mechanisch
Property | Value | Comment |
---|---|---|
Biegefestigkeit | 80 MPa Show Supplier Material materials with Biegefestigkeit of 80 MPa | ISO 178 |
Dehnung | 50 % Show Supplier Material materials with Dehnung of 50 % | min., ISO 527 |
Elastizitätsmodul | 2 GPa Show Supplier Material materials with Elastizitätsmodul of 2 GPa | ISO 527 |
Elongation at yield | 9 % Show Supplier Material materials with Elongation at yield of 9 % | ISO 527 |
Hardness, Ball Indentation | 80 MPa Show Supplier Material materials with Hardness, Ball Indentation of 80 MPa | ISO 2039-1 |
Härte, Shore D | 78 [-] Show Supplier Material materials with Härte, Shore D of 78 [-] | DIN 53505 |
Schlagfestigkeit, Charpy gekerbt | 22 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 22 kJ/m² | ISO 179 |
Schlagzähigkeit, Charpy ungekerbt | 252 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 252 kJ/m² | ISO 179 |
Streckgrenze | 50 MPa Show Supplier Material materials with Streckgrenze of 50 MPa | ISO 527 |
Thermisch
Property | Value | Pressure | Comment | ||
---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 0.00015 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 0.00015 1/K | DIN 53752 | |||
Max. Betriebstemperatur | 150 °C Show Supplier Material materials with Max. Betriebstemperatur of 150 °C | Longterm | |||
Long | |||||
Short | |||||
Min. Betriebstemperatur | -30 °C Show Supplier Material materials with Min. Betriebstemperatur of -30 °C | Longterm | |||
Vicat-Erweichungstemperatur | 138 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 138 °C | ISO 306, VST B50 | |||
Wärmeformbeständigkeitstemperatur | 104 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 104 °C | 2 MPa | |||
145 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 145 °C | 0.45 MPa | ||||
Wärmeleitfähigkeit | 0.13 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 0.13 W/(m·K) | DIN 52612 | |||
Entflammbarkeit | V-0 UL 94 |
Elektrisch
Property | Value | Comment |
---|---|---|
Dielektrizitätskonstante | 7 [-] Show Supplier Material materials with Dielektrizitätskonstante of 7 [-] | DIN 53483 |
Durchschlagfestigkeit | 27 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 27 kV/mm | VDE 0303 |
Kriechstromfestigkeit | 600 V Show Supplier Material materials with Kriechstromfestigkeit of 600 V | IEC 60112 |
Surface resistivity | 1e+10 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+10 Ω/sq | min., VDE 0303 |
Verlustfaktor | 0.24 [-] Show Supplier Material materials with Verlustfaktor of 0.24 [-] | DIN 53483 |
Volume resistivity | 1e+10 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+10 Ω·cm | min., VDE 0303 |
Technological properties
Property | ||
---|---|---|
Application areas | Chemical instruments, pipes and pumps | |
Certifications | RoHS,REACH |