Allgemein
Property | Value | Comment |
---|---|---|
Coefficient of friction | 0.35 [-] Show Supplier Material materials with Coefficient of friction of 0.35 [-] | DIN 53375, D, Against dry running steel |
Dichte | 1.15 g/cm³ Show Supplier Material materials with Dichte of 1.15 g/cm³ | ISO 1183 |
Wasserabsorption | 2.2 % Show Supplier Material materials with Wasserabsorption of 2.2 % | ISO 62 |
Mechanisch
Property | Value | Comment | |
---|---|---|---|
Biegefestigkeit | 140 MPa Show Supplier Material materials with Biegefestigkeit of 140 MPa | ISO 178 | |
Dehnung | 40 % Show Supplier Material materials with Dehnung of 40 % | ISO 527 | |
Elastizitätsmodul | 3 GPa Show Supplier Material materials with Elastizitätsmodul of 3 GPa | ISO 527 | |
Hardness, Ball Indentation | 160 MPa Show Supplier Material materials with Hardness, Ball Indentation of 160 MPa | ISO 2039-1 | |
Härte, Shore D | 82 [-] Show Supplier Material materials with Härte, Shore D of 82 [-] | DIN 53505 | |
Schlagfestigkeit, Charpy gekerbt | 4 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 4 kJ/m² | min., ISO 179 | |
Streckgrenze | 80 MPa Show Supplier Material materials with Streckgrenze of 80 MPa | ISO 527 | |
Schlagzähigkeit, Charpy ungekerbt | No break, ISO 179 |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 8e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 8e-05 1/K | DIN 53752 | |
Max. Betriebstemperatur | 105 °C Show Supplier Material materials with Max. Betriebstemperatur of 105 °C | Longterm | |
Long | |||
Short | |||
Min. Betriebstemperatur | -40 °C Show Supplier Material materials with Min. Betriebstemperatur of -40 °C | Longterm | |
Wärmeleitfähigkeit | 0.23 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 0.23 W/(m·K) | DIN 52612 | |
Entflammbarkeit | HB UL 94 |
Elektrisch
Property | Value | Comment |
---|---|---|
Dielektrizitätskonstante | 3.7 [-] Show Supplier Material materials with Dielektrizitätskonstante of 3.7 [-] | DIN 53483 |
Durchschlagfestigkeit | 50 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 50 kV/mm | VDE 0303 |
Surface resistivity | 1e+13 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+13 Ω/sq | min., VDE 0303 |
Verlustfaktor | 0.03 [-] Show Supplier Material materials with Verlustfaktor of 0.03 [-] | DIN 53483 |
Volume resistivity | 1e+15 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+15 Ω·cm | min., VDE 0303 |
Technological properties
Property | ||
---|---|---|
Application areas | Sliding parts, rollers and impact stressed parts | |
Certifications | Food Contact: FDA and EU 10/2011, RoHS,REACH |