Allgemein
Property | Value | Comment |
---|---|---|
Coefficient of friction | 0.12 [-] Show Supplier Material materials with Coefficient of friction of 0.12 [-] | DIN 53375, A, Against dry running steel |
Dichte | 0.96 g/cm³ Show Supplier Material materials with Dichte of 0.96 g/cm³ | max., ISO 1183 |
Wasserabsorption | 0.01 % Show Supplier Material materials with Wasserabsorption of 0.01 % | max. |
Mechanisch
Property | Value | Comment |
---|---|---|
Dehnung | 200 % Show Supplier Material materials with Dehnung of 200 % | min., ISO 527 |
Elastizitätsmodul | 0.7 GPa Show Supplier Material materials with Elastizitätsmodul of 0.7 GPa | min., ISO 527 |
Hardness, Ball Indentation | 30 MPa Show Supplier Material materials with Hardness, Ball Indentation of 30 MPa | min., ISO 2039-1 |
Härte, Shore D | 61 [-] Show Supplier Material materials with Härte, Shore D of 61 [-] | ISO 868 |
65 [-] Show Supplier Material materials with Härte, Shore D of 65 [-] | ISO 868 | |
Schlagfestigkeit, Charpy gekerbt | 80 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 80 kJ/m² | min., ISO 179 |
Streckgrenze | 20 MPa Show Supplier Material materials with Streckgrenze of 20 MPa | ISO 527 |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Max. Betriebstemperatur | 80 °C Show Supplier Material materials with Max. Betriebstemperatur of 80 °C | Longterm | |
Long | |||
Short | |||
Schmelzpunkt | 130 - 135 °C Show Supplier Material materials with Schmelzpunkt of 130 - 135 °C | ISO 3146 | |
Wärmeleitfähigkeit | 0.41 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 0.41 W/(m·K) | DIN 52612 | |
Entflammbarkeit | HB UL 94 |
Elektrisch
Property | Value | Comment |
---|---|---|
Surface resistivity | 1e+09 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+09 Ω/sq | max., IEC 60243 |
Volume resistivity | 1e+06 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+06 Ω·cm | max., IEC 60243 |
Technological properties
Property | ||
---|---|---|
Application areas | Sliding parts, chain guidance and sliding profiles | |
Certifications | Food Contact: FDA, RoHS,REACH | |
UV resistance | Partly |