Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 150 MPa Show Supplier Material materials with Biegefestigkeit of 150 MPa | ISO 178, 2 mm/min |
Biegemodul | 23.0 °C | 6 GPa Show Supplier Material materials with Biegemodul of 6 GPa | ISO 178, 2 mm/min |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 6 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 6 kJ/m² | ISO 180 |
Zugfestigkeit | 23.0 °C | 100 MPa Show Supplier Material materials with Zugfestigkeit of 100 MPa | ISO 527, 5 mm/min |
Thermisch
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Automotive structural parts (e.g. sunroof frames). | |
Certifications | RoHS,RECH | |
Color | Black | |
Fillers | 15% Glass Fiber and Mineral Powder | |
Processing methods |