Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.55 g/cm³ Show Supplier Material materials with Dichte of 1.55 g/cm³ | ASTM D792 |
Recycled Content | 45 % Show Supplier Material materials with Recycled Content of 45 % |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 150 MPa Show Supplier Material materials with Biegefestigkeit of 150 MPa | ISO 178, 2 mm/min |
Biegemodul | 23.0 °C | 5.9 GPa Show Supplier Material materials with Biegemodul of 5.9 GPa | ISO 178, 2 mm/min |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 6 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 6 kJ/m² | ISO 180 |
Zugfestigkeit | 23.0 °C | 105 MPa Show Supplier Material materials with Zugfestigkeit of 105 MPa | ISO 527, 5 mm/min |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Aschegehalt | 23.0 °C | 15 % Show Supplier Material materials with Aschegehalt of 15 % | ASTM D5630 | ||
Heat deflection temperature, 1.80 MPa | 200 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 200 °C | ISO 75 | |||
Entflammbarkeit | V0, V0 5VA for 3.2 mm sample UL94 |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dissipation factor, 1kHz | 23.0 °C | 2E-3 [-] Show Supplier Material materials with Dissipation factor, 1kHz of 2E-3 [-] | ASTM D150 |
Durchschlagfestigkeit | 23.0 °C | 37 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 37 kV/mm | ASTM D149, 1.6 mm, 500V/s in oil |
Volume resistivity | 23.0 °C | 1.00E+18 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+18 Ω·cm | ASTM D257 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Electrical components, appliances and structral applications. | |
Certifications | RoHS,RECH | |
Color | Black | |
Fillers | 15% Glass Fiber and Mineral Powder | |
Processing methods |