Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 2.1 - 2.8 g/cm³ Show Material materials with Dichte of 2.1 - 2.8 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Elastizitätsmodul | 23.0 °C | 50 - 70 GPa Show Material materials with Elastizitätsmodul of 50 - 70 GPa |
Härte, Knoop, HK2 | 23.0 °C | 400 - 480 [-] Show Material materials with Härte, Knoop, HK2 of 400 - 480 [-] |
Poissonzahl | 23.0 °C | 0.2 - 0.22 [-] Show Material materials with Poissonzahl of 0.2 - 0.22 [-] |
Schubmodule | 23.0 °C | 26.5 - 27 GPa Show Material materials with Schubmodule of 26.5 - 27 GPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Glasübergangstemperatur | 440 - 560 °C Show Material materials with Glasübergangstemperatur of 440 - 560 °C | |
Glühtemperatur | 470 - 640 °C Show Material materials with Glühtemperatur of 470 - 640 °C | |
Koeffizient der thermischen Ausdehnung | 300.0 °C | 3.2E-6 - 7.38E-6 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 3.2E-6 - 7.38E-6 1/K |
Vicat-Erweichungstemperatur | 460 - 840 °C Show Material materials with Vicat-Erweichungstemperatur of 460 - 840 °C | |
Wärmeleitfähigkeit | 23.0 °C | 0.96 - 1.2 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 0.96 - 1.2 W/(m·K) |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dielektrizitätskonstante | 23.0 °C | 4.1 - 6.7 [-] Show Material materials with Dielektrizitätskonstante of 4.1 - 6.7 [-] | at 1MHz |
Verlustfaktor | 23.0 °C | 0 - 0.01 [-] Show Material materials with Verlustfaktor of 0 - 0.01 [-] | at 1MHz |
Optisch
Property | Value |
---|---|
Brechungsindex | 1.47 - 1.52 [-] Show Material materials with Brechungsindex of 1.47 - 1.52 [-] |