Borosilicate Glass: Properties, Production and Applications

Known for its heat resistance and physical durability, borosilicate glass is useful in many applications mostly involved with temperature changes. The material owes its strength and resistance to its unique combination of silica, boric oxide, among various other oxides. The presence of boron oxide to replace some of the oxide components enhances the binding forces within the glass material.

Borosilicate glass properties

Low thermal expansion

With a thermal expansion coefficient of at least 3.2 x 10-6 1/K, pure borosilicate glass is significantly more resistant to temperature changes where other types of glass may become warped or deformed.

Its strength in thermal shock exposure makes the material suitable for laboratory heating and cookware. This characteristically low thermal expansion allows the material to maintain its integrity, even when transferred from a cold region (such as a refrigerator) to a hot area (like an oven) in seconds.

Modifications in the amount of its components may increase the thermal expansion coefficient to 7.38 x 10-6 1/K, but it is still much more resistant than ordinary soda-lime glass.

Other thermal properties of borosilicate glass include the following:

  • Annealing temperature = 470 - 640°C
  • Vicat softening temperature = 460 - 840°C
  • Transition temperature = 440 - 560°C

High material strength

Compared to similar glassware, borosilicate glass can withstand blunt force impact better. It has a Shear modulus of 26.5 – 27 GPa and Knoop hardness of 400 – 480 at 20°C.

Chemical stability

Borosilicate glass can withstand corrosion and breaking when exposed to acidic environments.

Production and processing

This special type of glass is produced from melting the following substances (with corresponding approximate composition): silica sand  (59.5%), boric oxide (21.5%), potassium oxide (14.4%), zinc oxide (2.3%), and trace amounts of calcium oxide and aluminium oxide.

Other variants – such as in cases wherein borosilicate glass is used as cookware – may change the silica composition to as high as 81%, depending on its intended use.

The melting process requires an exceedingly higher temperature than traditional glass production, owing to the material’s high transition temperature of up to 560°C.

Once the substrate has been produced, borosilicate glass may be processed in a number of ways depending on the application for the material. This glass material may be moulded or drawn into tubes, and processed into custom shapes and sizes.

Applications of borosilicate glass

Borosilicate glass has become useful in a wide variety of industries and applications, because of its physical and chemical properties.

Laboratory glassware

Borosilicate glass is popular as a base material for laboratory glassware, mainly because of the material’s chemical and thermal stability. Most of the modern beakers, flasks, and other glass receptacles designed for laboratory use are made of borosilicate glass.

Pharmaceutical glass tubing

Borosilicate glass is used for the manufacture of pharmaceutical containers like syringes, cartridges, vials and ampoules. The material is mostly chemically inert when in contact with most liquid medication products.

Cookware and kitchen implements

Owing to its remarkable thermal resistance, this glass material has found its way into kitchenware, particularly for cooking and baking. Popular cookware brands make use of borosilicate glass for baking dishes and glass cooking pots.

In addition, because of its low thermal expansion, this glass material is used for measuring cups and similar receptacles. Graduations labelled on the glass containers retain their accuracy because the material won’t warp when exposed to high temperatures.

Optical equipment

Due to the stability of borosilicate glass, it is a good material in fabricating slides and lenses for microscopes, telescopes, and other optical devices. Addition of doping agents may change the glass characteristics, such as optical absorption spectra.

Lighting technology

Lighting equipment requires glass receptacles and membranes that can withstand intense heat, and this is where borosilicate glass is extremely useful. Devices that use this glass type include HID lamps, modern high-powered flashlights, and studio spotlights.

Recent studies involve modifications in the chemical composition of borosilicate glass, through the addition of doping chemicals. Alteration in the photoluminescence spectra of the material is poised to become useful for solid state display, W-LED, and similar applications.

Quellen

Did you know?

Borosilicate glass has a very low thermal expansion coefficient so that it holds up well over a wide temperature range, making it suitable for applications such as in laboratory glassware and baking cookware. Explore borosilicate glass materials on Matmatch.

Anwendungsbereiche

Farm Buildings

Horticulture

Glass & Ceramics

Glass

Glass In Building

Glass Products

Building Elements

Elements Of Buildings In General

Walls

Partitions

Facades

Interior Lighting

Consumer Goods

Decorative Applications

Furniture

Healthcare

Medical Equipment

Injection Equipment

Radiographic Equipment

Medical Equipment General

Pharmaceutical Industry

Environment Health Safety

Fire Protection

General Fire Protection

Pollution Control Equipment

Pollution Control Equipment General

Fluid Systems

Fluid Storage

Fluid Storage General

Vessels

Mobile Vessels

Pressure Vessels

Pipelines

Water Pipelines

Flanges

Couplings & Joints

Other Pipeline Components

Water Treatment

Manufacturing

Chipless Working Equipment

Moulds

Hand-Held Tools

Pneumatic Tools

Industrial Furnaces

Electric Furnaces

Energy

Burners & Boilers

Boilers & Heat Exchangers

Heat Exchangers In Energy

Chemical Industry

Equipment For Chemical Industry

Heat Exchangers

Solar Energy

Solar Thermal

Electrical Insulation

Glass & Ceramic Insulation

Semiconductor Industry

Insulation

Insulators

Electrical Accessories

Fuses & Ocp

Rotating Machinery

Generators

Electronics

Electronic Components

Sensors

Electronic Tubes

Packaging

Containers

Tubes

Laser Equipment

Lasers

Communications

Fibre Optics

Fibre Optic Connector

Other Fibre Optic Equipment

Radar

Material Handling

Continuous Handling

Conveyors

Pneumatic Transport

Food Packaging

Packaging Material

Bottles & Jars

Distribution & Vending Machines

Textile Industry

Textile Auxiliary Materials

Food Industry

Food Industry Containers

Food Industry Equipment

Chemical Industry Production

Analytical Chemistry

Laboratory Equipment

Laboratory Ware

Chemical Analysis

Equipment For The Chemical Industry In General

Reaction Vessels

Reaction Columns

Oil & Gas Industry

Equipment For Petroleum & Natural Gas Industry

Equipment For Petroleum & Natural Gas Industries In General

Volumetric Equipment

Glass In Industrial Applications

Gauge Glasses

Installations In Buildings

Plumbing

Water Heating

Drainage Systems

Lighting In General

Exterior Building Lighting

Domestic

Commercial & Industrial Heating Appliances

Electric Heaters

Shop Fittings

Shop Fittings In General

Cosmetics

Pharmaceutical Packaging

Welding

Glass To Metal Seals

Fluorescent Lamps

Display Devices

Sterilization

Disinfectants & Antiseptics

Signal Intensifier

Optoelectronics

Optoelectronics General

Detectors

Wafer Production

Optics & Imaging

Photography

Photo Equipment & Projectors

Camera Parts

Cinematography

Alle anzeigen