Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 2.4 - 2.7 g/cm³ Show Material materials with Dichte of 2.4 - 2.7 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Elastizitätsmodul | 23.0 °C | 70 - 80 GPa Show Material materials with Elastizitätsmodul of 70 - 80 GPa |
Härte, Knoop, HK2 | 23.0 °C | 500 - 640 [-] Show Material materials with Härte, Knoop, HK2 of 500 - 640 [-] |
Härte, Vickers | 23.0 °C | 480 - 670 [-] Show Material materials with Härte, Vickers of 480 - 670 [-] |
Poissonzahl | 23.0 °C | 0.2 [-] Show Material materials with Poissonzahl of 0.2 [-] |
Schubmodule | 23.0 °C | 26 - 31.7 GPa Show Material materials with Schubmodule of 26 - 31.7 GPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Glasübergangstemperatur | 620 - 790 °C Show Material materials with Glasübergangstemperatur of 620 - 790 °C | |
Glühtemperatur | 610 - 800 °C Show Material materials with Glühtemperatur of 610 - 800 °C | |
Koeffizient der thermischen Ausdehnung | 300.0 °C | 3.38E-6 - 9.8E-6 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 3.38E-6 - 9.8E-6 1/K |
Vicat-Erweichungstemperatur | 820 - 1010 °C Show Material materials with Vicat-Erweichungstemperatur of 820 - 1010 °C | |
Wärmeleitfähigkeit | 23.0 °C | 0.91 - 1.1 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 0.91 - 1.1 W/(m·K) |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dielektrizitätskonstante | 23.0 °C | 6.1 - 7.7 [-] Show Material materials with Dielektrizitätskonstante of 6.1 - 7.7 [-] | at 1MHz |
Verlustfaktor | 23.0 °C | 0 - 0.01 [-] Show Material materials with Verlustfaktor of 0 - 0.01 [-] | at 1MHz |
spezifischer Widerstand | 23.0 °C | 0.13 - 0.14 Ω·m Show Material materials with spezifischer Widerstand of 0.13 - 0.14 Ω·m |
Optisch
Property | Value |
---|---|
Brechungsindex | 1.49 - 1.55 [-] Show Material materials with Brechungsindex of 1.49 - 1.55 [-] |