Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 2.4 - 2.5 g/cm³ Show Material materials with Dichte of 2.4 - 2.5 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Elastizitätsmodul | 23.0 °C | 70 GPa Show Material materials with Elastizitätsmodul of 70 GPa |
Härte, Knoop, HK2 | 23.0 °C | 510 - 710 [-] Show Material materials with Härte, Knoop, HK2 of 510 - 710 [-] |
Poissonzahl | 23.0 °C | 0.2 - 0.23 [-] Show Material materials with Poissonzahl of 0.2 - 0.23 [-] |
Schubmodule | 23.0 °C | 29.8 - 30 GPa Show Material materials with Schubmodule of 29.8 - 30 GPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Glasübergangstemperatur | 530 - 570 °C Show Material materials with Glasübergangstemperatur of 530 - 570 °C | |
Glühtemperatur | 530 - 560 °C Show Material materials with Glühtemperatur of 530 - 560 °C | |
Koeffizient der thermischen Ausdehnung | 300.0 °C | 8.3E-6 - 9.5E-6 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 8.3E-6 - 9.5E-6 1/K |
Vicat-Erweichungstemperatur | 720 - 730 °C Show Material materials with Vicat-Erweichungstemperatur of 720 - 730 °C | |
Wärmeleitfähigkeit | 23.0 °C | 0.7 - 1.3 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 0.7 - 1.3 W/(m·K) |
Optisch
Property | Value |
---|---|
Brechungsindex | 1.52 [-] Show Material materials with Brechungsindex of 1.52 [-] |